Epoxy flooring is often selected for a smooth, continuous appearance. That appearance says little about the concrete beneath it. When blisters, small holes or detached patches appear later, adding another coat of resin is not automatically the correct response.

First establish which defect is present and where it occurs in the assembly. Buildwise identifies residual moisture, a weak or contaminated surface layer and incorrectly treated joints among possible causes of resin-floor problems. [1] A photograph can show a symptom without proving the mechanism behind it.

Illustration of a garage with a smooth, glossy grey floor.
AI-generated illustration, not a photograph of a completed Montivo project.

A blister is not the same as a pinhole

Blistering involves a local area of the finish lifting. Delamination means that layers are no longer adequately bonded. Pores or pinholes are small surface openings that can develop during application. These defects should not be assigned one diagnosis without investigation.

Record when the defect appeared, its location and whether it is spreading. Keep information about the floor construction, previous treatments and applied products. Investigation may need to distinguish failure at an interface from failure within a weak substrate. They can look similar from above but require different treatment.

Use an appropriate moisture assessment

A surface that feels dry does not establish the moisture condition of the floor assembly. The test method, location, depth and selected resin system determine how a reading should be interpreted. Sika describes different methods and directs assessment back to the relevant product documentation. [2]

Avoid a universal moisture percentage without stating what it measures. An indicative reading is not automatically permission to coat. It is also necessary to distinguish residual moisture from moisture that may continue to enter later. Remmers likewise highlights professional moisture assessment before installation. [5]

A moisture-control layer is a solution only where it is approved for the actual conditions and complete flooring system. It should not become an automatic response to every unfavourable reading.

The coating needs a sound substrate

Dust, oil, old coatings and weak surface laitance can interfere with bonding to sound material. Preparation must therefore match the conditions found. Removing dust or applying a primer does not automatically make an insufficiently strong layer suitable.

Ask for the proposed mechanical preparation, cleaning and repairs to be described, together with how their result will be checked. Oil contamination may extend beyond what is visible. A trial area or targeted adhesion assessment may be needed to support the proposed method. Its extent follows the project conditions rather than a standard recipe for every garage.

Temperature and air can affect application

The dew point is the temperature at which moisture in the air can condense. A cold substrate in humid air therefore needs attention even when the room appears acceptable. The required margin above the dew point and permitted working conditions belong to the selected system’s documentation. [2]

Air can also escape from a porous substrate as it warms, leaving small openings. Sika describes this mechanism for application to porous substrates during rising temperatures. [3] This identifies a possible cause, not the explanation for every visible pore. Record substrate temperature and ambient conditions rather than looking only at the outdoor temperature.

Coordinate mixing, layers and joints

Epoxy is generally a reactive system: components react to form the final layer. Ratio, mixing procedure, working time and recoating interval belong to the particular product. Documentation for a two-component primer such as Sikafloor-161 illustrates how product-specific these requirements are. [4]

Do not transfer those values to another product or add improvised dilution outside the instructions. Cracks and joints also require a deliberate decision. A movement joint should not simply disappear beneath a seamless finish. Record which joints remain and which repairs must be completed before coating.

Safety documentation, personal protection and ventilation are part of work preparation. A short working time is not a reason to bypass them. The installation sequence should be organised around the approved conditions rather than relying on last-minute corrections.

Repair the cause before choosing the colour

For an existing damaged floor, first request a defined investigation. This may involve moisture assessment, a local opening through the assembly and checks of adhesion or substrate cohesion. Those findings then support a choice between local repair and more extensive removal.

Separate technical repair from the final visual result. A local repair may retain a colour, texture or sheen difference. Agree how the trial area and completed floor will be assessed. One new topcoat should not be promised as an invisible, permanent cure for every existing defect.

It is useful to keep a photographic record before any opening or removal. The condition of the exposed underside can provide information that is lost once the area is cleaned and repaired.

Keep useful handover information

Retain the system build-up, test results, product references and maintenance instructions. Ask when the floor can receive foot traffic, mechanical loading and the intended cleaning process. These stages need not occur at the same time.

Montivo can discuss the substrate condition and intended use before a resin floor is selected. A durable solution begins with verifiable preparation and a suitable system, not only an attractive finishing coat.

Sources and technical background

  1. Buildwise — Controle en voorbereiding van ondergronden: schilderwerk en harsvloeren (2026-03.06)
  2. Sika — Surface Prep Guide
  3. Sika — Sikafloor-82 EpoCem
  4. Sika — Sikafloor-161
  5. Remmers Belgium — Questions fréquemment posées sur les sols coulés

This article provides general considerations. Site assessment and the current requirements of the selected system determine the installation.